Online Repository of E-contents (ORE)

Deoxidation and strengthening of steels using Fe-Ti-C master alloy

Show simple item record

dc.contributor.author Malla, K.C.
dc.contributor.author Chakrabarti, A.K.
dc.contributor.author Galgali, R.K.
dc.date.accessioned 2018-10-01T12:20:48Z
dc.date.available 2018-10-01T12:20:48Z
dc.date.issued 1998
dc.identifier.citation Ironmaking & Steelmaking, 25(2), 1998: 168-172
dc.identifier.issn 0301-9233
dc.identifier.uri http://ore.immt.res.in/handle/2018/753
dc.description.abstract A Fe-Ti-C master alloy, prepared by carbothermic reduction of ilmenite ore in a transferred are plasma reactor, was tried out for deoxidation and dispersion strengthening of steels. Although it was not effective as a deoxidiser, it could be successfully used for impregnation of the ferrous matrix with dispersoids of TIC as well as for modification of sulphide and silicate inclusions. The TIC particles coarsened and gradually dissolved in austenite on raising the temperature to 1150 degrees C, but reprecipitated as submicroscopic particles during subsequent cooling. IS/1296 (C) 1998 The Institute of Materials.
dc.language en
dc.publisher Institute of Materials, Minerals and Mining
dc.relation.isreferencedby SCI
dc.rights Copyright [1998]. All efforts have been made to respect the copyright to the best of our knowledge. Inadvertent omissions, if brought to our notice, stand for correction and withdrawal of document from this repository.
dc.subject Materials Sciences
dc.subject Materials Sciences
dc.title Deoxidation and strengthening of steels using Fe-Ti-C master alloy
dc.type Journal Article
dc.affiliation.author IIT Kharagpur, Kharagpur-721302, West Bengal, India


Files in this item

Files Size Format View

There are no files associated with this item.

This item appears in the following Collection(s)

Show simple item record

Search Repository

Browse

My Account