Abstract:
The effect of Sn addition on the microstructure and corrosion behavior of squeeze-cast Mg-2Zn-1Ca alloys was investigated with 0 wt.%, 1 wt.%, and 2 wt.% Sn (ZX21, ZTX211, and ZTX221). A similar to 22% grain refinement and an increase in secondary phase fraction from 9.8% to 12.5% were achieved with 1 wt.% Sn, whereas 2 wt.% Sn promoted CaMgSn intermetallics alongside Mg2Ca and MgZn phases. Electrochemical tests revealed that ZTX211 exhibited the best performance, with corrosion current density nearly halved relative to ZX21 and markedly reduced long-term corrosion rates. In contrast, ZTX221 showed only moderate improvement due to microgalvanic coupling. SKPFM confirmed smoother potential transitions for ZTX211, correlating with its more uniform degradation. Thus, the optimized 1 wt.% Sn addition significantly enhanced corrosion resistance, identifying ZTX211 as a promising orthopedic implant material, subject to cytotoxicity and in vitro biocompatibility validation.