Kar, B.B.; Murthy, B.V.R.; Misra, V.N.
(International Journal Of Mineral Processing, 76(3), 2005: 143-147)
Spent hydro-refining catalysts mainly consists of 20-22% MoO3, 5-6% NiO, 4-5% S, 1-2% CO3O4, 1.3-1.5% Fe2O3, 3-4% SiO2, and the balance is Al2O3. In the present study, one such spent catalyst was roasted with sodium chloride ...