dc.contributor.author |
Rath, S.S. |
|
dc.contributor.author |
Rao, D.S. |
|
dc.date.accessioned |
2018-12-17T10:34:09Z |
|
dc.date.available |
2018-12-17T10:34:09Z |
|
dc.date.issued |
2017 |
|
dc.identifier.citation |
International Journal Of Minerals Metallurgy And Materials, 24(12), 2017: 1341-1351 |
|
dc.identifier.issn |
1674-4799 |
|
dc.identifier.uri |
http://ore.immt.res.in/handle/2018/2486 |
|
dc.description.abstract |
The present investigation examines the viability of dolochar, a sponge iron industry waste material, as a reductant in the reduction roasting of iron ore slimes, which are another waste generated by iron ore beneficiation plants. Under statistically determined optimum conditions, which include a temperature of 900A degrees C, a reductant-to-feed mass ratio of 0.35, and a reduction time of 30-45 min, the roasted mass, after being subjected to low-intensity magnetic separation, yielded an iron ore concentrate of approximately 64wt% Fe at a mass recovery of approximately 71% from the feed iron ore slime assaying 56.2wt% Fe. X-ray diffraction analyses indicated that the magnetic products contain magnetite and hematite as the major phases, whereas the nonmagnetic fractions contain quartz and hematite. |
|
dc.language |
en |
|
dc.publisher |
Springer |
|
dc.relation.isreferencedby |
SCI |
|
dc.rights |
Copyright [2017]. All efforts have been made to respect the copyright to the best of our knowledge. Inadvertent omissions, if brought to our notice, stand for correction and withdrawal of document from this repository. |
|
dc.subject |
Materials Sciences |
|
dc.subject |
Materials Sciences |
|
dc.subject |
Materials Sciences |
|
dc.subject |
Mining & Mineral Processing |
|
dc.title |
Dolochar as a reductant in the reduction roasting of iron ore slimes |
|
dc.type |
Journal Article |
|
dc.affiliation.author |
CSIR-Institute of Minerals and Materials Technology, Bhubaneswar 751013, Odisha, India |
|