Pradhan, S.K.; Das, J.; Rout, P.P.; Das, S.K.; Samantray, S.; Mishra, D.K.; Sahu, D.R.; Pradhan, A.K.; Zhang, K.; Srinivasu, V.V.; Roul, B.K.
(Journal Of Alloys And Compounds, 509(6), 2011: 2645-2649)
A clean signature of room temperature multiferroicity in Bi1.2Gd0.1Fe0.8O3 ceramics is observed. Samples were prepared by slow step sintering technique at 850 degrees C. Impurity peaks normally present in original BiFeO3 ...